Water uptake and release characteristics of PMMA cement containing the water-soluble contrast media iohexol or iodixanol have been investigated. The water uptake study revealed that iohexol had the highest uptake of water (3.7%) and that iodixanol had an uptake close to that of Palacos R (2.3% and 1.9%). The curves obtained showed the materials to follow classic diffusion theory, with an initial linearity with respect to t(1/2) making it possible to calculate the diffusion coefficients. This showed iohexol to have the lowest diffusion coefficient, Palacos R the highest, and iodixanol close to that of Palacos R. The release study showed that more iohexol than iodixanol was released from the bone cement; the long-term release was above 25 microg/mL for iohexol compared to slightly above 10 microg/mL for iodixanol. A microCT investigation showed that the risk of developing an observable radiolucent zone is negligible.
Medical subject headings
- Bone Cements
- Iodine
- Water