Reduction of wear volume from ultrahigh molecular weight polyethylene knee components by the addition of vitamin E.
biomechanical · Level V
Where this comes from
- Record sourced from PubMed, PMID 17975842.
- No licence information is recorded for this record.
- Because redistribution is not established, this page shows the abstract only. Follow the links below for the full text.
Abstract
Wear performance and debris-size distribution of vitamin E (DL-alpha tocopherol, VE)-added ultrahigh molecular weight polyethylene (UHMWPE) was evaluated using a knee-simulator test. VE was mixed with GUR 1050 UHMWPE powder at 0.3 wt%, and the tibial components of the knee joint were made by direct compression molding. The VE-added UHMWPE showed consistently lower wear volume throughout the test.