High-density polyethylene facial implants show surface oxidation in SEM and EDX examination: a pilot study.
case_series · Level IV
Where this comes from
- Record sourced from PubMed, PMID 19117817.
- Also identified by DOI 10.1016/j.actbio.2008.11.027.
- No licence information is recorded for this record.
- Because redistribution is not established, this page shows the abstract only. Follow the links below for the full text.
Abstract
Previous histopathological studies on explanted Medpor high-density polyethylene (HDPE) facial implants indicated signs of material destruction and claimed to observe phagocytized HDPE particles within the tissue samples beside the usual type IV reaction with severe fibrosis. We examined new and explanted Medpor material with scanning electron microscopy (SEM) and energy-dispersive X-ray analysis (EDX). The implant surface of three patient-derived specimens showed significantly higher oxygenation in EDX analysis and morphological changes in SEM compared to the new unused material directly after opening of the package and after 1 year of exposure to air. Our preliminary findings indicate a possible oxidative biocorrosion in HDPE surgical implants. Further studies should confirm these pilot project results.
Medical subject headings
- Polyethylene
- Prostheses and Implants
- X-Rays