As a way to modify both the physical and biological properties of a highly elastic and degradable polyurethane (PU), silk fibroin (SF) was blended with the PU at differing ratios. With increasing SF content, the tensile strength decreased as did the strain at break; the stiffness increased to around 35 MPa for the highest silk content. C2C12 (a mouse myoblast cell line) cells were used for in vitro experiments and showed significantly improved cell responses with increasing SF content. With increasing SF content the number of non-adherent cells was reduced at both 4 and 8h compared to the sample with the lowest SF content. In addition, muscle marker genes were upregulated compared to the sample containing no SF, and in particular sarcomeric actin and α-actin.
Medical subject headings
- Biocompatible Materials
- Cell Differentiation
- Elasticity
- Fibroins
- Myoblasts
- Polyurethanes