Corrosion on the acetabular liner taper from retrieved modular metal-on-metal total hip replacements.
case_series · Level IV
Where this comes from
- Record sourced from PubMed, PMID 24997654.
- Also identified by DOI 10.1016/j.arth.2014.05.027.
- No licence information is recorded for this record.
- Because redistribution is not established, this page shows the abstract only. Follow the links below for the full text.
Abstract
Eight retrieved metal-on-metal total hip replacements displayed corrosion damage along the cobalt-chromium alloy liner taper junction with the Ti alloy acetabular shell. Scanning electron microscopy indicated the primary mechanism of corrosion to be grain boundary and associated crevice corrosion, which was likely accelerated through mechanical micromotion and galvanic corrosion resulting from dissimilar alloys. Coordinate measurements revealed up to 4.3mm(3) of the cobalt-chromium alloy taper surface was removed due to corrosion, which is comparable to previous reports of corrosion damage on head-neck tapers. The acetabular liner-shell taper appears to be an additional source of metal corrosion products in modular total hip replacements. Patients with these prostheses should be closely monitored for signs of adverse reaction towards corrosion by-products.
Medical subject headings
- Acetabulum
- Arthroplasty, Replacement, Hip
- Hip Prosthesis
- Prosthesis Failure
Anatomy
- hip
- pelvis