We report the early failure of five ceramic-on-ceramic hip resurfacings (CoCHRs). The ceramic used for the acetabular liner was a novel ceramic-composite (two thirds polyurethane and one third alumina ceramic). All cases were revised for increasing metal ion levels (blood cobalt 3.93-208.0 μg/l and chromium 1.57-17.5 μg/l) due to ceramic liner fracture and/or accelerated wear of the ceramic femoral head coating. Patients underwent bearing exchange and revision using primary hip arthroplasty implants at a mean of 3.0 years following CoCHR. Intraoperatively all patients had metallosis. At 1 to 2 years of follow-up blood metal ions normalized with no complications. We do not recommend this particular type of ceramic-on-ceramic bearing for hip resurfacing.
Medical subject headings
- Arthroplasty, Replacement, Hip
- Hip Prosthesis
- Prosthesis Failure
Anatomy
- hip