Altering the concentration of silica tunes the functional properties of collagen-silica composite scaffolds to suit various clinical requirements.
basic_science · Level V
Where this comes from
- Record sourced from PubMed, PMID 25922091.
- Also identified by DOI 10.1016/j.jmbbm.2015.04.006.
- No licence information is recorded for this record.
- Because redistribution is not established, this page shows the abstract only. Follow the links below for the full text.
Abstract
The success of a tissue engineering scaffold depends on a fine balance being achieved between the physicochemical and biological properties. This study attempts to understand the influence of silica concentration on the functional properties of collagen-silica (CS) composite scaffolds for soft tissue engineering applications. Increasing the ratio of silica to collagen (0.25, 0.5, 0.75, 1.0, 1.25, 1.5 and 2.0 w/w) gave a marked advantage in terms of improving the water uptake and compressive modulus of the CS scaffolds, while also enhancing the biological stability and the turnover time. With increase in silica concentration the water uptake and compressive modulus increased concurrently, whereas it was not so for surface porous architecture and biocompatibility which are crucial for cell adhesion and infiltration. Silica:collagen ratio of ≤1 exhibits favourable surface biocompatibility, and any further increase in silica concentration has a detrimental effect.
Medical subject headings
- Biocompatible Materials
- Collagen Type I
- Silicon Dioxide
- Tissue Scaffolds