Contemporary Dual Mobility Head Penetration at Five Years: Concern for the Additional Convex Bearing Surface?
retrospective_cohort · Level III
Where this comes from
- Record sourced from PubMed, PMID 29602536.
- Also identified by DOI 10.1016/j.arth.2018.02.061.
- No licence information is recorded for this record.
- Because redistribution is not established, this page shows the abstract only. Follow the links below for the full text.
Abstract
Dual mobility (DM) bearings are increasingly popular and second-generation designs contain highly cross-linked polyethylene. The purpose of this study is to report head penetration rates in modern DM bearings. A review of 63 consecutive DM bearings was performed. Radiographs were analyzed for head penetration using Martell methodology at regular postoperative intervals. Thirty-four DM bearings were analyzed. Mean linear head penetration was 1.59 mm/y at 1 year, 1.07 mm/y at 2 years, and 0.27 mm/y at 5 years following an exponential regression model (R<sup>2</sup> = 0.999). Mean volumetric wear was 783 mm<sup>3</sup>/y at 1 year, 555 mm<sup>3</sup>/y at 2 years, and 104 mm<sup>3</sup>/y at 5 years following an exponential regression model (R<sup>2</sup> = 0.986). Initial head penetration of DM bearings is larger than contemporary cross-linked polyethylene bearings; however, rates approach steady state after 2 years, analogous to traditional bearings. The larger "bedding-in" head penetration may be due to the additional convex bearing surface, creating 2 surfaces for deformation/wear.
Medical subject headings
- Arthroplasty, Replacement, Hip
- Hip Prosthesis
- Prosthesis Design
Anatomy
- hip