Circumventing huge volume strain in alloy anodes of lithium batteries.
basic_science · Level V
Where this comes from
- Record sourced from PubMed, PMID 32284535.
- Also identified by DOI 10.1038/s41467-020-15452-0 and PMC identifier 7154030.
- Licence recorded as CC BY.
- The licence permits redistribution, so the abstract is shown in full and the full text is available from the publisher.
Abstract
Since the launch of lithium-ion batteries, elements (such as silicon, tin, or aluminum) that can be alloyed with lithium have been expected as anode materials, owing to larger capacity. However, their successful application has not been accomplished because of drastic structural degradation caused by cyclic large volume change during battery reactions. To prolong lifetime of alloy anodes, we must circumvent the huge volume strain accompanied by insertion/extraction of lithium. Here we report that by using aluminum-foil anodes, the volume expansion during lithiation can be confined to the normal direction to the foil and, consequently, the electrode cyclability can be markedly enhanced. Such a unidirectional volume-strain circumvention requires an appropriate hardness of the matrix and a certain tolerance to off-stoichiometry of the resulting intermetallic compound, which drive interdiffusion of matrix component and lithium along the normal-plane direction. This metallurgical concept would invoke a paradigm shift to future alloy-anode battery technologies.