Compressive Strength Testing of Glass-Fibre-Reinforced Tooth Crown Tissues After Endodontic Treatment.
biomechanical · Level V
Where this comes from
- Record sourced from PubMed, PMID 37794298.
- Also identified by DOI 10.1007/s10439-023-03377-w and PMC identifier 10808276.
- Licence recorded as CC BY.
- The licence permits redistribution, so the abstract is shown in full and the full text is available from the publisher.
Abstract
The objective of this study was to compare the effects of using short and continuous fibres for repairing compression-induced tooth crown damage. Human teeth were used for the study. They were upper medial incisors and maxillary first premolars lost due to periodontal causes. The teeth were divided into two groups with Hahnenkratt and short glass fibres. Teeth compressive strength tests were carried out. Then micro-CT imaging of the teeth and their fractures obtained after compression was performed. The teeth restored with Hahnenkratt's glass fibre posts showed higher compressive strength than the teeth restored using the EverX Posterior material. The tooth's most weakened and sensitive point after endodontic treatment was the cervical area of the tooth. All cracks were parallel to the root canal.
Medical subject headings
- Tooth Fractures
- Tooth, Nonvital