Interfacial Distortion of Sb<sub>2</sub>Te<sub>3</sub>-Sb<sub>2</sub>Se<sub>3</sub> Multilayers via Atomic Layer Deposition for Enhanced Thermoelectric Properties.
basic_science · Level V
Where this comes from
- Record sourced from PubMed, PMID 38919047.
- Also identified by DOI 10.1021/acsnano.3c13152 and PMC identifier 11238618.
- Licence recorded as CC BY.
- The licence permits redistribution, so the abstract is shown in full and the full text is available from the publisher.
Abstract
Atomic layer deposition (ALD) is an effective technique for depositing thin films with precise control of layer thickness and functional properties. In this work, Sb<sub>2</sub>Te<sub>3</sub>-Sb<sub>2</sub>Se<sub>3</sub> nanostructures were synthesized using thermal ALD. A decrease in the Sb<sub>2</sub>Te<sub>3</sub> layer thickness led to the emergence of distinct peaks from the Laue rings, indicative of a highly textured film structure with optimized crystallinity. Density functional theory simulations revealed that carrier redistribution occurs at the interface to establish charge equilibrium. By carefully optimizing the layer thicknesses, we achieved an obvious enhancement in the Seebeck coefficient, reaching a peak figure of merit (<i>zT</i>) value of 0.38 at room temperature. These investigations not only provide strong evidence for the potential of ALD manipulation to improve the electrical performance of metal chalcogenides but also offer valuable insights into achieving high performance in two-dimensional materials.