Abstract
Al impurity is among the most likely components to enter the spent lithium-ion battery (LIB) cathode powder due to the strong adhesion between the cathode material and the Al current collector. However, high-value metal elements tend to be lost during the deep removal of Al impurities to obtain high-purity metal salt products in the conventional hydrometallurgical process. In this work, the harmful Al impurity is designed as a beneficial ingredient to upcycle high-voltage LiCoO<sub>2</sub> by incorporating robust Al-O covalent bonds into the bulk of the cathode assisted with Ti modification. Benefiting from the strong Al-O and Ti-O bonds in the bulk, the irreversible phase transitions of the upcycled R-LCO-AT have been significantly suppressed at high voltages, as revealed by in situ XRD. Moreover, a Li<sup>+</sup>-conductive Li<sub>2</sub>TiO<sub>3</sub> protective layer is constructed on the surface of R-LCO-AT by pinning slow-diffusion Ti on the grain boundaries, resulting in improved Li<sup>+</sup> diffusion kinetics and restrained interface side reactions. Consequently, the cycle stability and rate performance of R-LCO-AT were significantly enhanced at a high cutoff voltage of 4.6 V, with a discharge capacity of 189.5 mAhg<sup>-1</sup> at 1 C and capacity retention of 92.9% over 100 cycles at 4.6 V. This study utilizes the detrimental impurity element to upcycle high-voltage LCO cathodes through an elaborate bulk/surface structural design, offering a strategy for the high-value utilization of spent LIBs.