Etching-Free Dual Lift-Off for Direct Patterning of Epitaxial Oxide Thin Films.
basic_science · Level V
Where this comes from
- Record sourced from PubMed, PMID 40774799.
- Also identified by DOI 10.1021/acs.nanolett.5c02947.
- No licence information is recorded for this record.
- Because redistribution is not established, this page shows the abstract only. Follow the links below for the full text.
Abstract
Although monocrystalline oxide films offer broad functional capabilities, their practical use is hampered by challenges in patterning. Traditional patterning relies on etching, which can be costly and prone to issues like film or substrate damage, underetching, overetching, and lateral etching. In this study, we introduce a dual lift-off method for direct patterning of oxide films, circumventing the etching process and associated issues. Our method involves an initial lift-off of amorphous Sr<sub>3</sub>Al<sub>2</sub>O<sub>6</sub> or Sr<sub>4</sub>Al<sub>2</sub>O<sub>7</sub> (<i>a</i>SAO) through stripping the photoresist, followed by a subsequent lift-off of the functional oxide thin films by dissolving the <i>a</i>SAO layer. <i>a</i>SAO functions as a "high-temperature photoresist", making it compatible with the high-temperature growth of monocrystalline oxides. Using this method, patterned ferromagnetic La<sub>0.67</sub>Sr<sub>0.33</sub>MnO<sub>3</sub> and ferroelectric BiFeO<sub>3</sub> were fabricated, accurately mirroring the shape of the photoresist. Our study presents a straightforward, flexible, precise, environmentally friendly, and cost-effective method for patterning high-quality oxide thin films.